Metal Sheet Slitting Blade

Metal Sheet Slitting Blade

Metal Sheet Slitting Blade is mainly used in coiling machine for metal sheet like mild steel, stainless steel, Aluminum, Copper, galvanized sheet and cold or hot rolled plate trimming and slitting.

We have manufacturing capability of production slitting knife size up to 650mm at OD with material Cr12MoV. D2. W6Mo5Cr4V2. W18Cr4V, H13. H13K. H13Ni. HMB. LD. DC53. Thickness tolerance within 0.001 mm and flatness within 0.0015mm could be assured accordingly; Advanced heat treatment and strict inspection make sure our knifes superior and stable quality.

Metal Sheet Slitting Blade 1

Metal Working Blades

Our industrial shearing blades are built to handle the toughest metal cutting tasks. From hydraulic guillotines to CNC shear machines, our blades provide a sharp, reliable cut on heavy-plate materials. Forged from shock-resistant tool steels and heat-treated for maximum toughness, these shearing knives are designed to resist chipping and deformation, significantly extending the intervals between regrinds.

First-class industrial blades to optimize your printing productivity.

In addition to a comprehensive product range in the field of high-performance knives and spare parts for the metal sheet slitting blade, we convince through creative and technical competence, service readiness and direct personal contact. We support your process optimization for best printing results and a longer service life.

Due to our own research and development department we meet your requirements for:

  • Optimized material quality
  • Efficient lamella shapes
  • Specific treatment procedures
  • Innovative coatings

whilst developing, manufacturing and delivering.

Metal Sheet Slitting Blade

Shearing machine blades are often made of high- and medium-carbon alloy steel materials.  The material has poor thermal conductivity, low plasticity, high deformation resistance, and a narrow forging temperature range (about 200°C).  In order to achieve deep forging, the tonnage of the forging hammer should be appropriately selected.  If the tonnage is too small, the deformation will only occur on the surface, and the quality of the core of the forging blank cannot be improved;  if the tonnage is too large, the impact will be too heavy, and it will easily crack.

During the forging process, light blows should be made at the beginning and end of forging, and heavy blows in the middle.  During the forging process, pay attention to the uniform deformation of each part and maintain the uniform temperature of each part;  pay attention to multi-directional upsetting;  pay attention to ensuring a sufficient forging ratio.  , the total forging ratio is generally 8 to 18, and the single forging ratio is generally 2 to 3.  If 5 to 10 is used, the effect will be better.

Commonly used materials are: Cr12MoV, D2, W6Mo5Cr4V2, W18Cr4V, H13, , LD. DC53 etc.

The thickness tolerance can be guaranteed to be within 0.001mm and the flatness to be within 0.0015mm;  advanced heat treatment and strict inspection ensure the excellent and stable quality of our cutting tools.

Medium and high alloy steel shearing blades such as Cr12MoV. H13, due to the increase in alloy elements inside the blade, a large amount of alloy carbides are formed during quenching.  During the cooling process, they have high hardenability, so more residual austenite will be obtained.  Body structure, only through 3-4 times of high-temperature tempering can the untransformed Parasite be transformed into martensite and increase the hardness of the blade.  Insufficient tempering of the blade is also a defect in which the hardness does not meet the requirements.  The martensite quenched structure is not fully transformed into tempered martensite, and the residual austenite still exists in the matrix.  Since the residual austenite has good plasticity and toughness, it will cause Insufficient hardness.  Therefore multiple temperings are crucial for blades made of high alloy materials!

9crsi steel is a high-carbon low-alloy steel tool steel with good tempering resistance.  Because of its economical material, it is often used to make shearing blades.  It is suitable for cutting ordinary plates, low-alloy plates, and stainless steel plates below 1.2mm.  Shearing slightly thicker plates shows insufficient toughness and is prone to chipping and failure.  Jiaheng blades are summarized through long-term production practice.  The zero-insulation toughening process for quenching this steel type can eliminate the early failure caused by conventional heating, oxidation and decarburization of the blade.  Uneven austenite quenching can refine the martensite.  After quenching, cryptocrystalline martensite or fine Acicular martensite, this structure has better strength and toughness!  It greatly increases the cutting thickness range of the blade and adds real economic benefits to customers!

LD steel contains a large amount of alloying elements and has many varieties, and its alloying is more complicated. Steel has poor thermal conductivity and high austenitization temperature, so the heating process should be slow, and preheating or step heating is often used.

In order to protect the surface quality of steel, the heating medium should be paid attention to, so advanced heating equipment and methods of controlled atmosphere furnaces are commonly used. Salt bath heating should be fully deoxidized and purified, and air furnace heating must be protected by paint.

On the premise of achieving the purpose of quenching, a gentler cooling method should be used.

LD mold steel is expensive, the shear blade processing is complex, the cycle is long, and the manufacturing cost is high. Therefore, the process formulation and operation should be very cautious to avoid quality accidents and ensure the safety of the entire production process.

DC53 (Cr8Mo2VSi) is a new type of cold work die steel improved from SKD11. It has a carbon content of 1%, 8% chromium, 2% molybdenum, V 0.28% Si 0.9%. It has extremely high wear resistance and excellent toughness after heat treatment. It is a Class medium carbon alloy steel! After quenching 1020-1040, tempering at 520-530℃ can still ensure HRC62-63, which overcomes the shortcomings of Cr12MoV’s insufficient hardness and poor toughness after high-temperature tempering. The toughness is twice that of Cr12MoV. D2, and its cutting and grinding properties are better. Well, there is no risk of cracking during wire cutting. After tempering, Paralympic is almost completely transformed, and cryogenic treatment is basically unnecessary. Tempering at a low temperature of 200°C, the carbides are evenly distributed, and there are no massive carbides in the structure.

Shearing machine blades are used in many varieties, small batches, and the overall shearing blade is extremely long (≥4m). Therefore, it is more appropriate to use a box furnace for quenching. However, during the heating process of the blade in the box furnace, due to the effect of the surrounding oxidizing atmosphere, oxidative decarburization will occur, causing the surface of the blade to lose its metallic luster and increase its roughness. The oxidation will reduce the strength of the steel and its mechanical properties, and the decarburization will be significantly reduced. The quenching hardness, wear resistance and fatigue performance of the blade, the oxidation and decarburization of silicon steel such as 9SiCr.60Si2Mn in the blade material are particularly obvious! Therefore, surface protection of the blade before quenching is very important!

Due to excessive dimensional deformation of the heat treatment length of long blades, the assembly accuracy will be reduced or even scrapped. Process measures to control the change in the length of the overall ultra-long cutting blade: First, the source of raw materials ① Oxide, sulfide ≤ level 2, loose center, generally loose ≤ level 2 , 100mm of the material head part is not allowed to be cut. ② Avoid cold hammering correction during forging. The local plastic deformation caused by hammering and straightening on the surface will cause lengthwise shortening due to stress relaxation during quenching and heating. ③The annealed structure of the knife blank should be uniform spherical pearlite. ④ Take measures to improve the hardenability and ensure the stability of the quenching medium, and eliminate or reduce the reduction in hardenability caused by oxidative decarburization during the heating process!

ShengDuan blades, quality comes from every detail!

The material of the blade determines the length of its heating time. The general rule is that the heating time is from long to short: high-speed steel and high-alloy steel > low-alloy tool steel > high-carbon steel > low-carbon steel. The reason is that the carbon and alloy elements reduce The thermal conductivity of the material, and the alloying elements accelerate the structural transformation of the steel. In addition, the alloy carbides are relatively stable, and the diffusion coefficient is smaller than that of carbon and iron, which slows down the diffusion of carbon in the steel, so the holding time must be appropriate. Extension, the size and shape of the blade also have a certain impact on the heating time, and the furnace loading method and furnace loading volume cannot be ignored.

During the shearing blade grinding process, due to the cutting, scoring and frictional effects of the abrasive grains on the blade, the metal surface is plastically deformed, and the relative displacement between the metal molecules inside the blade generates internal friction and heat; when the grinding wheel is cutting, relative to The speed of the blade is very high, causing severe external friction with the blade surface to generate heat. And because the cutting of each abrasive is instantaneous, the heat is generated instantaneously and cannot be dissipated in time, so the instantaneous temperature in the grinding area Higher, generally reaching 800~1500℃. If the heat dissipation measures are not good, it is easy to cause burns on the blade surface, that is, secondary quenching and high-temperature tempering will occur on the surface of the blade (generally tens to hundreds of microns). , destroying the structure on the blade surface and seriously reducing the service life of the blade!

At the same time, discuss the importance of the mounting holes for the shearing blades: the shearing blades are fixed on the upper and lower knife seats through special cup-head (counterbore) screws to ensure the stability of the gap between the upper and lower shearing blades and subsequent adjustment, and the blade counterbore angle The precision of the hole directly affects the pressing force of the fitting surface of the cup nut. During the shearing process, the cutting edge is subject to strong friction and extrusion force. The axial direction of the cutting edge is caused by insufficient pressing force of the screw fitting surface. Insufficient resistance causes gap jump, resulting in premature failure of the burrs of the sheared sheet and the shearing edge! ShengDuan blades, we speak with experience!

During the use of the shearing machine blades, excessive consumption may occur due to discomfort during operation, which increases the cost of using the shearing machine. First, the gap between the upper and lower blades should be adjusted within the range of 0.05-0.1mm/mm according to the thickness and strength of the material being sheared! A gap that is too small will increase the number of shears, and a gap that is too large will not only produce the same problem, but will also result in an excessively large bevel. During the shearing process, the blade will generate strong squeezing and friction. After a period of use, the metal molecules on the surface of the blade will be arranged out of order, generating internal stress and fatigue sources, causing the blade to become dull and causing burrs to appear on the cross section of the material being sheared. A dull cutting edge will reduce the rated shearing capacity by 50%, causing the machine tool to be overloaded, and may also cause the blade to break, etc.! It is recommended that users frequently observe and inspect, perform sharpening in a timely manner, and use a tempering furnace to eliminate stress at low temperature before sharpening the blade if possible! ShengDuan blade, we have been guiding customers to create value!

About Shengzhong

Maanshan ShengZhong Heavy Industry Machinery Co., Ltd. is a professional industrial blade manufacturer of development, production and sales.
The company has a professional technical team, perfect processing equipment, mature production technology.

Introduction

We are a manufacturer of industrial blades. With a professional design and production team, we can provide you with a complete solution.

Service

We are highly specialized in manufacturing custom industrial blades and machine knives per sample and drawing.

History

Since 1990.We always put our old customers first and provide the best service.

Our Team

We have more standard size machine knives and industrial blades available directly from stock。Also accept OEM/ODM

Contact Us
You can reach us by telephone at +86 153 8555 2696 and by e-mail at: jon.szblade@gmail.com
In a hurry? Then use the following contact form and we will get back to you!

Like what you see? Get in touch today.

You can get in touch with us via email or the phone. Simply complete the form, upload any image you may have and we will be in touch within 2 business working days.

Scroll to Top

Get a Custom Quote

We use cookies to enable all functionalities for best performance during your visit and to improve our services by giving us some insight into how the website is being used. Continued use of our website without having changed your browser settings confirms your acceptance of these cookies. For details please see our privacy policy.